Austenitic Stainless Steel |
Cast Alloy Designation | CG8M |
UNS Number | J93000 |
|
Comparable Wrought Alloy | 317 |
Applicable ASTM Spec | A351/A743 |
|
|
Chemical Composition |
C | 0.08 |
Mn | 1.5 |
Si | 1.5 |
P | 0.04 |
S | 0.04 |
Cr | 18.0 - 21.0 |
|
Ni | 9.0 -13.0 |
Mo | 3.0 - 4.0 |
Fe | --- |
Cu | --- |
Other | --- |
|
|
Mechanical Properties |
Tensile (ksi) | 75 |
Yield (ksi) | 35 |
Elongation (%) | 25 |
|
Reduction of area (%) | --- |
Hardness (Brinell) | 162 -220 |
|
|
Notes |
All single values are maximums unless noted otherwise.
Brinell hardness values and ranges represent typicals for the grade. |
More Info |
Weldable | Yes |
Castability | Good |
Processability | Good |