Heat Resistant Stainless Steel |
Cast Alloy Designation | HW | UNS Number | N08001 |
| Comparable Wrought Alloy | --- | Applicable ASTM Spec | A297 |
|
|
Chemical Composition |
C | 0.35 - 0.75 | Mn | 2 | Si | 2.5 | P | 0.04 | S | 0.04 | Cr | 10.0 -14.0 |
| Ni | 58.0 - 62.0 | Mo | 0.50 | Fe | --- | Cu | --- | Other | --- |
|
|
Mechanical Properties |
Tensile (ksi) | 60 | Yield (ksi) | --- | Elongation (%) | --- |
| Reduction of area (%) | --- | Hardness (Brinell) | 185 |
|
|
Notes |
All single values are maximums unless noted otherwise.
Brinell hardness values and ranges represent typicals for the grade. |
More Info |
Weldable | Yes |
Castability | Good |
Processability | Good |