Nickel Base |
Cast Alloy Designation | ILLIUM GX | UNS Number | --- |
| Comparable Wrought Alloy | Hastelloy X | Applicable ASTM Spec | A567 |
|
|
Chemical Composition |
C | 0.02 | Mn | 1 | Si | 1 | P | 0.04 | S | 0.03 | Cr | 20.5 - 23.0 |
| Ni | --- | Mo | 8.0 -10.0 | Fe | 17.0 - 20.0 | Cu | --- | Other | Co 0.5 - 2.5W 0.2 -1.0, Fe 17.0 - 20.0 |
|
|
Mechanical Properties |
Tensile (ksi) | 55 | Yield (ksi) | 35 | Elongation (%) | 8 |
| Reduction of area (%) | --- | Hardness (Brinell) | 179 |
|
|
Notes |
All single values are maximums unless noted otherwise.
Brinell hardness values and ranges represent typicals for the grade. |
More Info |
Weldable | Yes |
Castability | Medium |
Processability | Medium |