Ductile Ni-Resist |
Cast Alloy Designation | NiResist D4 | UNS Number | F43005 |
| Comparable Wrought Alloy | --- | Applicable ASTM Spec | A439 |
|
|
Chemical Composition |
C | 2.6 | Mn | 1.00 | Si | 5.00-6.00 | P | 0.08 | S | --- | Cr | 4.50-5.50 |
| Ni | 28.00-32.00 | Mo | --- | Fe | --- | Cu | --- | Other | --- |
|
|
Mechanical Properties |
Tensile (ksi) | 60 | Yield (ksi) | --- | Elongation (%) | --- |
| Reduction of area (%) | --- | Hardness (Brinell) | 202-273 |
|
|
Notes |
All single values are maximums unless noted otherwise.
Brinell hardness values and ranges represent typicals for the grade. |
More Info |
Weldable | Yes but need special acceptance from customer |
Castability | Good |
Processability | Good |